JPH0149317B2 - - Google Patents
Info
- Publication number
- JPH0149317B2 JPH0149317B2 JP58161050A JP16105083A JPH0149317B2 JP H0149317 B2 JPH0149317 B2 JP H0149317B2 JP 58161050 A JP58161050 A JP 58161050A JP 16105083 A JP16105083 A JP 16105083A JP H0149317 B2 JPH0149317 B2 JP H0149317B2
- Authority
- JP
- Japan
- Prior art keywords
- coal tar
- tar
- solid content
- content
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Coke Industry (AREA)
- Working-Up Tar And Pitch (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16105083A JPS6051783A (ja) | 1983-08-31 | 1983-08-31 | バインダ−の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16105083A JPS6051783A (ja) | 1983-08-31 | 1983-08-31 | バインダ−の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6051783A JPS6051783A (ja) | 1985-03-23 |
JPH0149317B2 true JPH0149317B2 (en]) | 1989-10-24 |
Family
ID=15727649
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16105083A Granted JPS6051783A (ja) | 1983-08-31 | 1983-08-31 | バインダ−の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6051783A (en]) |
Families Citing this family (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103965931B (zh) * | 2013-01-31 | 2016-01-20 | 北京宝塔三聚能源科技有限公司 | 一种改质沥青的制备方法 |
CN104232130B (zh) * | 2013-06-09 | 2016-08-10 | 任相坤 | 一种针状焦的生产工艺 |
CN104232136B (zh) * | 2013-06-09 | 2016-08-10 | 任相坤 | 一种用于生产针状焦的原料沥青的处理工艺 |
CN104232143B (zh) * | 2013-06-09 | 2016-08-10 | 任相坤 | 一种生产针状焦的工艺 |
CN108102692B (zh) * | 2016-11-25 | 2019-11-15 | 中国石油化工股份有限公司 | 一种煤基原料生产针状焦的工艺方法 |
CN108102712B (zh) * | 2016-11-25 | 2019-11-15 | 中国石油化工股份有限公司 | 一种混合原料生产针状焦的组合工艺方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57209989A (en) * | 1981-06-18 | 1982-12-23 | Kawasaki Steel Corp | Preparation of coal tar pitch |
JPS581783A (ja) * | 1981-06-27 | 1983-01-07 | Nippon Steel Chem Co Ltd | ピツチの製造法 |
-
1983
- 1983-08-31 JP JP16105083A patent/JPS6051783A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6051783A (ja) | 1985-03-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3018242A (en) | Production of hydrogen-enriched hydrocarbonaceous liquids | |
JP2005325364A (ja) | 高効率蒸発蒸留方法を用いたコールタール及び炭化水素混合ピッチ製品 | |
CN109370628B (zh) | 一种煤系针状焦的生产工艺 | |
US3240566A (en) | Method of obtaining maximum separability of organic matter from ash in coal extraction processes | |
US3928169A (en) | Production of pitch substantially soluble in quinoline | |
US3251751A (en) | Process for carbonizing coal | |
JPH0150354B2 (en]) | ||
US4663022A (en) | Process for the production of carbonaceous pitch | |
JPS6149355B2 (en]) | ||
JPH0149317B2 (en]) | ||
JPH0149316B2 (en]) | ||
JPH09100473A (ja) | 高炉用コークス製造方法 | |
CN113457204B (zh) | 利用焦化粗苯萃取煤直接液化油渣的方法 | |
JPS61197688A (ja) | 石炭系重質物の精製方法 | |
KR101359266B1 (ko) | 석탄 피치 제조 방법 | |
CN109370627B (zh) | 一种用于制备高品质煤系针状焦的溶剂、制备方法及其应用 | |
US4582591A (en) | Process for the separation of resinous substances from coal-base heavy oils and use of the fraction obtained | |
JPH0149315B2 (en]) | ||
KR102498310B1 (ko) | 함침 피치의 제조 방법 | |
CN109370630B (zh) | 一种制备煤系针状焦原料的方法 | |
JP2000008047A (ja) | 高炉用コークス製造方法 | |
JPH10204441A (ja) | 含浸用ピッチの製造方法およびその製造装置 | |
RU2075496C1 (ru) | Способ получения нефтяного пека | |
CN109370631B (zh) | 一种最大化利用煤焦油生产煤系针状焦的生产方法 | |
EP4603564A1 (en) | Process to obtain synthetic pitches with high softening point from medium and heavy aromatic oils |